What is the temperature for adding early strength agent to concrete?
The temperature for adding early strength agent to concrete should not be lower than -5 ℃. When the daily temperature is within the range of 0 to 5 ℃, early strength agents can be employed, but insulation measures must be adopted. The specific temperature requirements should also be adjusted in accordance with the construction environment …